90 g/m² per ISO 536 Test Method, (24 lbs)
|
|
124 microns/4.9 mil per ISO 534 Test Method
|
|
89% per TAPPI T-425 Test Method
|
|
89% per TAPPI T-452 Test Method
|
|
117 per CIE Ganz 82 Test Method
|
|
|
|
15 to 30° C / 59 to 86° F
|
|
|
Display permanence (Indoor home or office)
|
4+ years behind glass indoor away from direct with HP 727 Inks4
|
Display permanence (Commercial in window)
|
1+ month with HP 727 Inks with or without lamination5
|
|
Immediate (at 23° C, 50% RH)
|
|
Yes, compatible with thermal, heat assist, and pressure-sensitive film laminates
|
|
2 years, unopened in original packaging
|
|
5 to 40° C / 41 to 104° F
|
|
|
|
Recyclable through commonly available recycling programs
|
|
|